- 16
- Mar
Detailed use steps of epoxy resin pipe
Detailed use steps of epoksie hars pyp
1. Use dry cotton cloth or sandpaper to remove dust, oil stains, rust, etc. on the bonding surface, and then wipe with a cleaning agent such as acetone or trichloroethylene to clean the bonding surface.
2. Fully stir evenly in proportion to use; in order to ensure the effect of use, it can also be mixed in vacuum.
3. Use up within the operable time range, otherwise it will solidify and cause waste of materials.
4. After gluing, it will be cured at room temperature for 2-6 hours; at 40℃ it will be cured for 1-3 hours; ten days after sizing, the adhesion will be better. It needs to be heated to 15-25℃ for indoor use.