Tushen dalilin shigar coil ƙonewa
Tushen dalilin shigar coil ƙonewa
Ƙunƙarar murɗar induction shine saboda rufin ya lalace, kuma ingancin insulator kai tsaye yana shafar ƙimar amfani da tanderun narkewa da amincin yanayin aikin ma’aikaci. Duk da haka, abin takaici ne cewa rufi na induction coils bai sami isasshen kulawa ba a cikin masana’antu. Yawancin masana’antun kawai suna fesa fenti na al’ada na fenti a matsayin abin rufe fuska bayan an yi nada. Yawancin irin wannan nau’in fenti mai rufewa shine kwayoyin halitta. Abun yana da insulating mai kyau a dakin da zafin jiki, amma yayin da zafin jiki ya tashi, aikin wannan nau’in insulating varnish yana raguwa da sauri, kuma shi kansa yana da carbonized a hankali. Lokacin da zafin jiki ya wuce 100 ° C, varnish mai rufewa zai zama cikakke carbonized kuma ya yi baki. , Rashin rufin asiri.