Comparison of wear resistance of different materials and induction heating processes
Comparison of wear resistance of different materials and induction heating processes
Craft
Gatunek stali |
Ogrzewanie indukcyjne | Lead bath heating | ||
twardość
HRC |
Abrasion/
(10 _7g/km) |
twardość
HRC |
Abrasion/
(10-7g/km) |
|
xnumxmnxnumx | 46 ~ 48 | 13.8 | 45 ~ 47 | 39.9 |
35CrNi3A | 52 ~ 53 | 3.8 | 52-53 euro | 4.4 |
45 Kr | 56-57 euro | 3. 1 | 56 ~ 58 | 3.9 |
T7A | 62 ~ 63 | 2. 8 | 63 ~ 65 | 2.5 |