site logo

Tsarin narkewa na aluminum-Copper master alloy induction narkewa tanderu

Tsarin narkewa na aluminum-Copper master alloy induction narkewa tanderu

1. Cikakken preheat da aka shirya cajin;

2. Cika tanderun da 10-15% aluminum da duk jan karfe. Yayin da jan karfe ya narke, sai a zuba sauran ingots na aluminium a cikin tanderun a cikin batches, sannan a jujjuya su sosai har sai sun narke;

3. Add refining wakili a game da 700 ℃ (adadin da aka kara bisa ga bukatun daban-daban refining jamiái, kamar AWJ-3 refining wakili, adadin kara ne 0.5-0.8%) ga degassing da refining, da slag an cire. kuma ana zuba ingot (ingot Thickness≤25mm).