How to detect the lining thickness of a high-temperature electric furnace?
How to detect the lining thickness of a високотемпературна електрическа пещ?
1. Капацитивен метод
Методът на капацитета е подобен на метода на съпротивлението. Коаксиален кръгъл кондензаторен сензор е вграден вътре в облицовката на пещта, а стойността на капацитета съответства на неговата дължина. Дебелината на зидарията на доменната пещ може да се определи чрез измерване на стойността на капацитета.
2. Stress wave method
The stress wave signal is very sensitive to structural defects. When the stress wave propagates in the medium, such as holes, cracks and other interface discontinuities, reflection, refraction, scattering and mode conversion will occur. The thickness of the stave material can be determined.
3. Метод на съпротива
The resistance element is embedded inside the furnace lining, the front of the sensor is aligned with the inner surface of the furnace lining, and it is connected to the measurement system through a lead wire. The resistance value of the resistance element is related to its length. As the resistance element and the furnace lining lose synchronously, the resistance will change. Use the corresponding measurement The meter measures the electrical signal output by the component, and then the remaining thickness of the furnace lining can be measured online.
4. Метод за откриване на топлинен поток
Според термодинамиката температурната разлика, топлопроводимостта и дебелината на стената на пещта определят интензитета на топлинния поток. За облицовката на доменната пещ топлопроводимостта е фиксирана, а дебелината на стената на пещта може да се получи от температурната разлика и интензитета на топлинния поток.
The heat flow detection sensor is installed in the lower temperature part of the furnace lining. The heat flow intensity is calculated by the water temperature difference of the cooling wall of the hearth, and the temperature value measured by the thermocouple in the brick lining is combined to calculate the thickness of the furnace wall.
5. Ултразвуков метод
The thickness measurement is carried out at the point where the ultrasound propagates in the solid medium. At a constant temperature, the ultrasound is incident on the furnace lining and enters the furnace. The propagation time of the incident and reflection of the ultrasound in the furnace lining is used to obtain the residual thickness of the furnace lining.
6. Метод на термодвойка с много глави
Several thermocouples of different lengths are installed in a protective sleeve, and then they are installed in the brick lining that needs to be inspected, and the erosion of the masonry can be inferred by measuring the temperature change of each thermocouple. When the temperature of each point and the temperature gradient between each point are basically stable, when the brick lining is gradually eroded to a certain part, the galvanic couple in that part will be destroyed, and the temperature signal will be abnormal.
7. Метод на извод за модел
Той използва термодвойки като елементи за откриване, прилага термодинамика и други теории за установяване на математически модел на мястото на температурата на огнището и дъното на пещта и изчислява приблизителните позиции на линията за втвърдяване на разтопено желязо и линията на ерозия на въглеродни тухли чрез софтуерно програмиране и числен анализ.