- 18
- Dec
Molybdenum lanthanum alloy Njirimara: Kedu ihe dị iche n’etiti molybdenum lanthanum (Mo-La) alloy na TZM molybdenum alloy?
Molybdenum lanthanum alloy Njirimara: Kedu ihe dị iche n’etiti molybdenum lanthanum (Mo-La) alloy na TZM molybdenum alloy?
Kedu ihe dị iche n’etiti molybdenum lanthanum (Mo-La) alloy na TZM molybdenum alloy?
Kedu ihe bụ molybdenum-lanthanum alloy? Molybdenum-lanthanum alloy bụ alloy nke mebere isi metal molybdenum na lanthanum trioxide dị ugbu a dị ka irighiri ihe gbasasịrị na matriks. Ọdịnaya nke La2O3 na alloy bụ n’ozuzu 0.5% ~ 5.0% (oke ntakiri). Iji
Site na nyocha na arụmọrụ dị elu nke okpomọkụ na usoro kwekọrọ na molybdenum-lanthanum alloy na TZM alloy na 1000 ~ 1800 ℃. Nsonaazụ gosiri na mgbe okpomọkụ dị ala karịa 1400 ℃, molybdenum-lanthanum alloy nwere a elu keukwu arụmọrụ nke ike na plasticity. Mgbe okpomọkụ karịrị ma ọ bụ hà nhata 1400 ℃, ike tensile nke molybdenum-lanthanum alloy na-ebelata, na plasticity nke molybdenum-lanthanum alloy na-ebelatakwa. Site na mmụba nke okpomọkụ ule, ike nkwụsị nke TZM alloy na-ebelata, ma plasticity nke TZM molybdenum alloy na-abawanye, nke bụ kpọmkwem ihe na-emegide molybdenum-lanthanum alloy.
N’otu oge ahụ, ma ọ bụ ike ma ọ bụ plasticity, TZM alloy tụnyere molybdenum-lanthanum alloy n’otu okpomọkụ. Nleba anya na microstructure na-egosi na ihe abụọ a molybdenum alloys na-amalite recrystallize na 1100 ℃ ma na-aga n’ihu na 1550 ℃, na ọka ha recrystallized na-egosi elongated Ọdịdị, nke dị iche na equiaxed grains na recrystallized ala nke dị ọcha molybdenum.
1. Okwu mmalite nke molybdenum lanthanum alloy
Molybdenum lanthanum alloy, nke a makwaara dị ka molybdenum okpomọkụ dị elu, ika MoLa, bụ nke molybdenum doped na obere mkpụrụ nke lanthanum trioxide (La2O3) iji mepụta ihe a na-akpọ nhazi eriri laminated. Nkịta microstructure a pụrụ iche nwere ike ịnọgidesi ike ọbụlagodi na okpomọkụ dị elu 2000ºC. Ya mere, molybdenum-lanthanum oxide nwere nguzogide na-akpụ akpụ ọbụlagodi n’ọnọdụ oke ojiji. Anyị na-ahazi ụdị alloys molybdenum n’ime akụkụ ọkụ dị oke ọkụ, dị ka ọta ọkụ na-ekpo ọkụ na-ekpo ọkụ, ụgbọ mmiri na-ekpo ọkụ na mgbakasị ahụ, wires ndị tọrọ atọ ma ọ bụ mkpuchi evaporator.
2. Uru nke molybdenum lanthanum alloy:
Okpomọkụ recrystallization dị elu;
The elongated urughuru Ọdịdị nwere ike melite ductility;
Nguzogide oxidation siri ike;
Nguzogide na-akpụ akpụ dị elu.
3. Recrystalization okpomọkụ: 1400 ℃ ~ 1500 ℃.
4. Resistivity nke molybdenum-lanthanum alloy (otu: Ω * mm2/m)
okpomọkụ ℃ | 20 | 600 | 1000 | 1200 | 1400 | 1700 | 1800 | 1900 | 2000 |
Nguzogide | 0.054 | 0.205 | 0.314 | 0.374 | 0.435 | 0.506 | 0.525 | 0.558 | 0.571 |
5. Molybdenum lanthanum alloy mejupụtara
ọkwa | isi mgwa ihe% | (ọ dịghị ihe karịrị%) | |||||||||
Mo | Ti | Zr | C | Ike2 | C | 0 | N | Fe | Ni | Si | |
Mo1 | oke | – | – | – | – | 0.01 | 0.007 | 0.002 | 0.01 | 0.002 | 0.01 |
OZI | oke | 0.40 ~ 0.55 | 0.06 ~ 0.12 | 0.01 ~ 0.04 | – | – | 0.03 | 0.002 | 0.01 | 0.005 | 0.005 |
MoLa | oke | – | – | – | 0.4 ~ 1.2 | 0.01 | – | 0.002 | 0.01 | 0.002 | 0.01 |
6, Na-atụ aro elu ibu nke molybdenum-lanthanum alloy: 4 ~ 9W / cm2