Apa 45 # baja kudu tempered?

Apa 45 # baja kudu tempered?

Kebutuhan kanggo tempering tambahan ditemtokake dening kahanan. Yen tempering suhu ampas bisa dikontrol sajrone quenching, ora perlu tambahan tempering suhu rendah.

Struktur lan sifat baja 45 # sawise annealing, normalizing, quenching lan tempering.

45 # baja anil: ferit + pearlit;

45 # baja normalizing: ferit + pearlite;

45 # baja quenching: martensite;

45# baja tempering: martensit tempered (tempering suhu rendah), troostite tempered (tempering suhu medium), sorbite tempered (tempering suhu dhuwur).

Struktur baja 45 # sawise normalisasi yaiku struktur ferit + pearlit, struktur sawise quenching yaiku struktur martensit, lan struktur sawise quenching + 400 ℃ tempering minangka struktur troostite tempered. Kekerasan kinerja normalisasi kurang saka HB200, nanging materi kasebut gampang diproses, sing isih dadi rencana proses utama. Quenching +400 ℃ atose tempering apik banget, ndhuwur HB300.

Atose 45 # baja quenched lan tempered antarane HRC20 ~ HRC30;

Ing atose quenching saka 45 # baja antarane HRC55 ~ 58, lan Nilai bisa tekan HRC62;

Butuh 15-20 dina kanggo 45 # baja digunakake amarga mbutuhake perawatan tuwa kanggo stabil kinerja baja.

Kekerasan paling dhuwur ing aplikasi praktis yaiku HRC55 (frekuensi quenching HRC58).

45 # baja punika baja struktural karbon kualitas dhuwur karo atose kurang lan Processing nglereni gampang. Biasane digunakake ing cetakan minangka template, tips, kiriman pandhuan, lan liya-liyane, nanging perawatan panas dibutuhake