Methods to improve the effectiveness of gas blowing at the bottom of ladle
Methods to improve the effectiveness of gas blowing at the bottom of ladle
DW series slit type breathable brick
We have analyzed the process of argon blowing at the bottom of the ladle and the requirements for breathable bricks. This article focuses on methods to improve the effectiveness of gas blowing at the bottom of the ladle.
1. Choose better quality cigle koje dišu
The corrosion resistance and erosion resistance of breathable bricks are inseparable from the effect of the bottom blowing process. It has been learned from practice that after long-term use, traditional slit-type air-permeable bricks will be blocked by slit steel infiltration and slag build-up on air-permeable bricks. At this time, the blow-open rate of the air-permeable brick and the blow-through rate at the bottom of the ladle are naturally difficult to meet the requirements of ladle metallurgy.
Choosing air-permeable bricks with high thermal shock resistance, permeability resistance and erosion resistance is the first step to improve the bottom blowing effect of the ladle.
The slit width, the geometry of the slit, and the wettability of the ventilating core material to molten steel also affect the permeability of the ventilating brick. Therefore, when a long life is required, the impermeable ventilating brick Become a better choice.
2. Determine the appropriate bottom blowing gas pressure process parameters
According to the data, the minimum bottom blowing gas pressure is equal to the sum of the gas pressure on the liquid surface, the pressure loss of the gas supply pipeline, the additional pressure formed by bubbles, and the static pressure of the molten steel and the slag layer.
If the bottom blowing gas pressure is too small, the bubbles will be difficult to form or the stirring will be too weak.
Ako je pritisak plina za upuhivanje na dnu previsok, to će rezultirati smanjenjem agregacije i disperzije mjehurića, smanjenjem iskorištavanja plina za upuhivanje s donje strane i prekomjernog miješanja rastopljenog čelika, zbog čega je rastopljeni čelik previše u kontaktu s atmosferom tokom okretanja. , što rezultira pogoršanom sekundarnom oksidacijom rastaljenog čelika i velikim padom temperature.
The quality of different steel grades determines different steelmaking processes. The most suitable bottom blowing pressure is to meet the steelmaking process’s requirements for gas agitation strength, so that the steel liquid level will roll within an appropriate level, and the inclusions will float up to the greatest extent. At the same time, it can best play the role of ladle covering agent, better ensure that the covering agent absorbs the inclusions carried by air bubbles, and improve the purity of molten steel. In order to more accurately determine the most suitable bottom blowing gas pressure process parameters, a pressure gauge and a flow meter can be installed on the bottom blowing gas pipeline, and the bottom blowing gas pressure and gas supply volume can be determined according to different ladle parameters and metallurgical requirements.
u zakljucku
Da bi se poboljšao učinak upuhivanja plina na dnu lonca, odabir visokokvalitetnih prozračnih opeka s visokom otpornošću na termički udar, otpornošću na propusnost i otpornošću na eroziju je prvi korak. Odnos između naučne upotrebe i visokokvalitetne prozračne cigle može se opisati kao komplementaran